Mechanical Properties Metric English Comments
Flexural Strength 540 MPa
78300 psi
ASTM F417
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..