POLYMER SEARCH
Polymer Property : Flexural Strength = 5320 psi
Polymer Property :
Flexural Strength =
5320 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Strength
36.7
MPa
5320
psi
ASTM D790
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (Cond)