Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 36.5 MPa | 5290 psi | 1.0 in/min; 0.125" thickness; ASTM D-790 |
Chevron Phillips K-Resin® KR03BR SBC
(discontinued **) K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle.. |