Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 36.3 MPa | 5260 psi | ASTM D790 |
I. Stern HIPS SH03 High Impact Polystyrene Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc. |
|||
Flexural Strength | 36.3 MPa | 5260 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 36.3 MPa | 5260 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 36.3 MPa @Thickness 3.20 mm |
5260 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SH 03 High Impact Polystyrene Characteristics High flow Good melt strength Excellent toughness Processing MoldingApplications Gas assisted injection molding of T.V. cabinets Suitable for thin walled parts, AC grills and toys .. |