Mechanical Properties Metric English Comments
Flexural Strength 36.2 MPa
5250 psi
ASTM D790
Quadrant EPP PROTEUS® EURO-GRAY Copolymer Polypropylene
Flexural Strength 36.2 MPa
5250 psi
ASTM D790
Chase Plastics CP Pryme® N300HSL (COND, 50% RH) Nylon 6 (Utility Grade), Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 36.2 MPa
5250 psi
ASTM D790
Chase Plastics CP Pryme® N300L (COND, 50% RH) Nylon 6 (Utility Grade), Internally Lubricant
Information provided by Chase Plastics.