Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 359 MPa | 52000 psi | ASTM D790 |
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry Product Description: Glass Fiber (60% Reinforced), Nylon 6 injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents, Lubricants and Heat Stabiliz.. |
|||
Flexural Strength | 359 MPa @Temperature 23.9 °C |
52000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 120 Aramid Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Flexural Strength | 359 MPa | 52000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF55 HS L BK 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |