Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 356 MPa | 51600 psi | ASTM D790 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Strength | 356 MPa | 51600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Flexural Strength | 356 MPa | 51600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |
|||
Flexural Strength | 356 MPa | 51600 psi | |
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride Uniform, large sized pressed sintered aluminum nitride. |