Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.0 MPa | 5070 psi | ASTM D790 |
CPC - Vycom SEABOARDâ„¢ Premier High density polyethylene (HDPE) Seaboard High Density Polyethylene (HDPE) is the toughest marine grade polymer sheet available. This UV stable product has scratch resistance, excellent impact, and stiffness, yet it is easy to mach.. |