Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 3.30 MPa | 479 psi | |
Multibase Multi-Flex® TPE A 8699 BLK Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by.. |