Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 303 MPa @Temperature 23.9 °C |
44000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-601 Polyester Prepreg, 18oz. Woven Fiberglass Roving P-601 Polyester is a fire retardant prepreg resin system, which meets the requirements of MIL-R-7575. P-601 prepregs are available on any style of woven fiberglass fabric having a suitable finish, s.. |
|||
Flexural Strength | 303 MPa | 44000 psi | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF40 RM HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer Features: Heat Stabilized and Low Moisture AbsorptionAppearanc.. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES HiFill® PA6/12 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 50% Filler by WeightAppearance: Black and Natural ColorTPCI# 9814104Information provided by TP Composites, .. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES HiFill® PET GF55 X 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF33 ML2 BK 33% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 33% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceAp.. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF40 TL10 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat StabilizedInformation p.. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Chase Plastics CP Pryme® NN343L (Dry) Nylon 66, 43% Glass Fiber Reinforced, Lubricated, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
PolyOne Edgetek® PI-30CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 303 MPa | 44000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR-N BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |