Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS) Information provided by PolyOne |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 43 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Strength | 296 MPa @Temperature 23.0 °C |
42900 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Flexural Strength | 296 MPa @Strain 3.20 % |
42900 psi @Strain 3.20 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 296 MPa | 42900 psi | 5 mm/min; ISO 178 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 296 MPa | 42900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |
|||
Flexural Strength | 296 MPa @Temperature 23.0 °C |
42900 psi @Temperature 73.4 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Flexural Strength | 296 MPa | 42900 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific) LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Strength | 296 MPa | 42900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu.. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific) LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM F417 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | 296 MPa | 42900 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Flexural Strength | 296 MPa @Temperature 23.0 °C |
42900 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific) LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON PX06419 PA 6 LNP* VERTON* PX06419 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, Structural. |
|||
Flexural Strength | 296 MPa | 42900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON PX06419 PA 6 (Asia Pacific) LNP* Verton* PX06419 is a compound based on Nylon 6 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |