Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized Nylon 6, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES Luriblend® PA4/6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: LubricatedTPCI# 8661150Information provided by TP Composites, .. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Asahi Kasei Thermylon® LSG-440A-H 60% Ceramic and Glass Fiber Reinforced, Heat Information provided by Asahi Thermofil |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Asahi Kasei Thermylon® NSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |