Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Asia Pacific) LNP* Thermocomp* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA6.10 LNP* LUBRICOMP* QCP36 is a compound based on Nylon 6/10 resin containing 15% PTFE/Silicone, 30% Carbon Fiber. Added features of this material include: Wear Resistant. Electrically Conductive |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10 LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant. |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OE006 PPS - Linear LNP* STAT-KON* OE006 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear LNP* THERMOCOMP* OC006 is a compound based on PPS-Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific) LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. |
|||
Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti.. |