Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 280 MPa | <= 40600 psi | ISO 178 |
Polykemi AB SCANMID 6 B12^ F45 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 280 MPa | 40600 psi | |
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA (Asia Pacific) LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment... |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Flexural Strength | 280 MPa @Strain 3.50 % |
40600 psi @Strain 3.50 % |
ISO 178 |
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica.. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East) LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive. |
|||
Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are .. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber Heat stabilized 35% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
Tisan TISSAN® Flame Retardant (V0) Styrene Acrylonitrile Properties:Natural or ColoredGlass fiber and glass beadMineral filledFlame retardantGood thermal and chemical resistanceExcellent transparencyExcellent mechanical propertiesDimensional stabilityEasy.. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
Polyram PlusTek RA304G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 280 MPa | 40600 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Flexural Strength | >= 280 MPa | >= 40600 psi | cold bending |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Flexural Strength | 280 MPa | 40600 psi | at max force; ISO 178 |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Flexural Strength | >= 280 MPa | >= 40600 psi | cold bending |
China-Yixing Longly Refractories 75 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:.. |