Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 21.4 MPa | 3100 psi | ASTM D790 |
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Flexural Strength | 21.4 MPa | 3100 psi | ASTM D790 |
Quadrant EPP TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet) |
|||
Flexural Strength | 21.4 MPa @Temperature 1500 °C |
3100 psi @Temperature 2730 °F |
Parallel |
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |