Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.07 MPa | 300 psi | Burst Strength |
Saint-Gobain COHRlastic® 1010 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Flexural Strength | 2.07 MPa | 300 psi | Burst Strength |
Saint-Gobain COHRlastic® 3010 Low Temperature Flexibility Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Flexural Strength | 2.07 MPa | 300 psi | Parallel to thickness |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |