Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 190 MPa @Temperature 22.8 °C |
27500 psi @Temperature 73.0 °F |
ASTM D790 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Polymer Resources AC-G25 Acetal Copolymer, 25% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2240MGHL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement -15% Filler by Weight, Mineral -25% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Techmer ES Electrablend® PA6 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Techmer ES Electrablend® PA6 GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
Flexural Strength | 190 MPa | 27500 psi | ASTM D790 |
PolyOne Edgetek® ES-30GF/000 PES (Polyethersulfone), 30% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |