Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 166.28 MPa | 24117 psi | ASTM D790 |
E-Polymers SEPAZ® N1040 Nanoclay 4% High Flow Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |