Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 161 MPa | 23300 psi | Crosswise; ASTM D-790 |
Glastic 1130 Angles, Channels, and Structural Shapes Information provided by Glastic Corporation |
|||
Flexural Strength | 161 MPa | 23300 psi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 161 MPa | 23300 psi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 161 MPa | 23300 psi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 161 MPa | 23300 psi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 161 MPa | 23300 psi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 161 MPa | 23300 psi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 161 MPa | 23300 psi | Crosswise; ASTM D-790 |
Glastic GLASGUARD 1130 Corrosion-Resistant Panels GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corr.. |