Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 158.6 MPa | 23000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 158.6 MPa | 23000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 159 MPa @Temperature 23.9 °C |
23000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D790 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Flexural Strength | 159 MPa @Temperature 23.9 °C |
23000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D790 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
PolyOne Edgetek® AS-30CF/000 UV Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued Description/Features:Carbon Fiber ReinforcedUV StabilizedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Haysite H320 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF18 IM 511 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M35 HS BK 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by Weight and Mineral Filler, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Plastics Group Polifil® 930L-13GF Glass Fiber-Reinforced Nylon 6 (DAM) Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 159 MPa | 23000 psi | |
Anderman Ceramics EM60 Mullite Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics. |
|||
Flexural Strength | 159 - 186 MPa | 23000 - 27000 psi | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |