Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 156.96 MPa | 22765 psi | |
Shinil Chemical SHINCON PSU-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | |
Shinil Chemical SHINSTRA PBT SBV1015 Structural Polymer Lamp Housing SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | ASTM D790 |
E-Polymers SEPAZ® N1140 Nanoclay 4% Medium Viscosity Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | ASTM D790 |
E-Polymers SEPAZ® V200L Unfilled PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | ASTM D790 |
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | ASTM D790 |
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | ASTM D790 |
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Flexural Strength | 156.96 MPa | 22765 psi | ASTM D790 |
E-Polymers SEPAZ® LH30 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |