Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 150 MPa | 21800 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Flexural Strength | 150 MPa | 21800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66 Non-Hal red phosphorous based Flame Retardant CompoundAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Flexural Strength | 150 MPa | 21800 psi | ASTM D790 |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Flexural Strength | 150 MPa | 21800 psi | ASTM D790 |
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo.. |
|||
Flexural Strength | 150 - 180 MPa | 21800 - 26100 psi | Compression; ISO 178 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Flexural Strength | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-8052/EM/BL PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Flexural Strength | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1850-7952 PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Flexural Strength | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 50-0789 Polycarbonate, with carbon fiber, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Flexural Strength | 150 MPa | 21800 psi | ASTM D790 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Strength | 150 MPa | 21800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Flexural Strength | 150 MPa | 21800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Flexural Strength | 150 MPa | 21800 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Flexural Strength | 150 MPa | 21800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Flexural Strength | 150 MPa | 21800 psi | ASTM D790 |
Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled 30% low friction mineral filled polyamide 6.6 lubricated with molybdenum for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Polyram RamTough PZ324G4NT Polycarbonate, 20% Glass Fiber, Flame Retardant 20% glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178-93 |
Wellman EcoLon® MRGF1878-BK1 Nylon 6, 30% Mineral/Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Strength | 150 MPa | 21800 psi | cond; ISO 178 |
DSM Novamid® 1010GN8-30 NAT PA6-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free |
|||
Flexural Strength | 150 MPa @Temperature 23.0 °C |
21800 psi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 150 MPa | 21800 psi | 2 mm/min; ISO 178 |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Flexural Strength | 150 MPa | 21800 psi | ASTM D790 |
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Polyplastics Duracon® KT-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 150 MPa | 21800 psi | ISO 178 |
Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |