Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1390 MPa | 202000 psi | Bending Strength; 4-Point; DIN ENV 843-1 |
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2 DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications. |