Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 138 MPa | 20000 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Flexural Strength | 138 MPa | 20000 psi | |
Haysite 14200 Polyester BMC, 15% Glass Reinforced The 14200 series bulk molding compound is one of Haysite's newest molding compound families. This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional a.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Strength | 138 MPa | 20000 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Flexural Strength | 138 MPa | 20000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 NAT Availability: North AmericaForms: PelletsAppearance: Natural ColorTPCI# 8384101Information provided by TP Composites, Inc. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Plastics Group Polifil® 628-13GF Glass Fiber-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Chase Plastics CP Pryme® PC120GR Polycarbonate, 20% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Ensinger Tecapeek® XP-110 Compression Molded PEEK Compound, 45% Mineral Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Adell AT-13 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Adell BR-13 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 138 - 207 MPa @Strain 5.00 % |
20000 - 30000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 685 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.48% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Strength | >= 138 MPa | >= 20000 psi | |
Bulk Molding Compounds BMC 845 30% Glass Filled Vinyl Ester BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compressive creep at .. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Adell AT-33 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |