Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 131 MPa | 19000 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 131 MPa | 19000 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 131 MPa | 19000 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 131 MPa | 19000 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 131 MPa @Temperature 23.9 °C |
19000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D790 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
PolyOne Lubri-Tech™ PI-10CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Strength | 131 MPa | 19000 psi | |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES Electrablend® PA6/6 IM C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES Electrablend® PA6/PC Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 131 MPa | 19000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES Plastiblend® TPX-HTN-000BB Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D 790 |
SABIC Innovative Plastics Noryl GFN2L PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Strength | 131 MPa | 19000 psi | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Flexural Strength | 131 - 159 MPa | 19000 - 23000 psi | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Asahi Kasei Thermylene® P7-30FG-1804 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Flexural Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided.. |