Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 120 MPa | 17400 psi | STN EN ISO 178 |
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I.. |
|||
Flexural Strength | <= 120 MPa | <= 17400 psi | ISO 178 |
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 120 - 160 MPa | 17400 - 23200 psi | Injection; ISO 178 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Flexural Strength | 120 - 160 MPa | 17400 - 23200 psi | Injection; ISO 178 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 120 MPa | 17400 psi | |
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High.. |
|||
Flexural Strength | 120 MPa | 17400 psi | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Flexural Strength | 120 MPa | 17400 psi | 2mm/min; ASTM D790 |
Kingfa PA6-T25 25% Mineral Filled PA6 Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Flexural Strength | 120 MPa | 17400 psi | 2mm/min; ISO 178 |
Styron Pulse® 979 PC/ABS PULSE™ 979 is a high performance, 10% glass filled PC/ABS resin.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
Flexural Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat. |
|||
Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
Polyram PlusTek PB507 Nylon 6, Flame Retardant Flame retardant halogen free polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
Polyram PlusTek RA601 Nylon 6.6, Heat Resistant Heat resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
Polyram RamTough PZ303G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | >= 120 MPa | >= 17400 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.Information provided by Hippe. |
|||
Flexural Strength | 120 MPa | 17400 psi | |
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
Flexural Strength | 120 MPa | 17400 psi | ISO Data |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Flexural Strength | 120 MPa | 17400 psi | STN EN ISO 178 |
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |
|||
Flexural Strength | 120 MPa | 17400 psi | ISO 178, 2 mm/min |
Lucite International SW Sanitary Ware Acrylic Sheet Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International |
|||
Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |