Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 119 MPa | 17300 psi | 2mm/min; ASTM D790 |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
Global Atron 6601-B General Purpose Nylon 66 Information provided by Global Polymers Corporation. |
|||
Flexural Strength | 119 MPa | 17300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Strength | 119 MPa | 17300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific) 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Flexural Strength | 119 MPa | 17300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF10 L 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS LNP* THERMOCOMP* AF006XXZ is a compound based on ABS resin containing 30% Glass Fiber. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006 PA 66 LNP THERMOCOMP* RZ006 is a compound based on Nylon 66 resin containing 30% Milled Glass. |
|||
Flexural Strength | 119 MPa | 17300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66 LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
SABIC Innovative Plastics NORYL EFN4230 PPE+PS (Asia Pacific) PPE+PS high heat transparent grade |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
Plenco 1586 Polyester, Pellet, Transfer Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Flexural Strength | 119 MPa | 17300 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Flexural Strength | 119 MPa | 17300 psi | 2mm/min; ASTM D790 |
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 119 MPa | 17300 psi | ISO 178 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 124 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 134 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
Plenco 1510 Polyester, Granular, Transfer Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Flexural Strength | 119 MPa | 17300 psi | ASTM D790 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |