Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Plaskolite Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 108 MPa | 15700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790M |
DSM Somos® 7120 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific) LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 108 MPa | 15700 psi | ISO 178 |
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Techmer ES HiFill® PA6 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionTPCI# 9586102Information provided by TP Composites, Inc. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Techmer ES HiFill® PA6 HS L BK Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Techmer ES Plastiblend® PA6 HS L MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantHeat Stabilized and LubricatedTPCI# 7018102Information provided by TP Composites, Inc. |
|||
Flexural Strength | 108 MPa | 15700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 108 MPa | 15700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 108 MPa | 15700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 108 MPa | 15700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Flexural Strength | 108 MPa | 15700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 108 MPa | 15700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 108 MPa | 15700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 108 MPa | 15700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ISO 178 |
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Strength | 108 MPa | 15700 psi | ISO 178 |
Cathay PA56 Renewable Engineering Polyamide, DAM Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 108 MPa | 15700 psi | Wet; ASTM D790 |
Asahi Kasei Leona® 14G15 15% Glass Filled Nylon 66 15% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Heater tanks, fuel injectors, ABS sensors, and other under-the-hood automotive parts Information provided by Asahi Kasei |
|||
Flexural Strength | 108 MPa | 15700 psi | Dry; ASTM D790 |
Asahi Kasei Leona® 9400S Nylon 66 Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
Plaskolite West Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |