Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast UF3 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast UF4 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flexural Strength | 105.1 MPa | 15250 psi | ASTM D790 |
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |