Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 104 MPa | 15100 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 104 MPa | 15100 psi | X, Y direction; Condition A; ASTM D790 |
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Flexural Strength | 104 MPa | 15100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Flexural Strength | 104 MPa | 15100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Flexural Strength | 104 MPa | 15100 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Flexural Strength | 104 MPa | 15100 psi | ASTM D790 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Strength | 104 MPa | 15100 psi | ASTM D790 |
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Flexural Strength | 104 MPa | 15100 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® TS4016 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 104 MPa | 15100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Flexural Strength | 104 MPa | 15100 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific) PPO/PS unfilled high heat |
|||
Flexural Strength | 104 MPa | 15100 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 104 MPa | 15100 psi | at rupture; ASTM D790 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Strength | 104 MPa | 15100 psi | ASTM D790 |
Chase Plastics CP Pryme® N320GL (COND, 50% RH) Nylon 6 (Utility Grade), 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 104 MPa | 15100 psi | ISO 178 |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Strength | 104 MPa | 15100 psi | ISO 178 |
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Flexural Strength | 104 MPa | 15100 psi | ISO 178 |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Flexural Strength | 104 MPa | 15100 psi | Method 1, 0.05"/min; ASTM D790 |
Proto3000 PC Fused Deposition Modeling Polymer Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating .. |
|||
Flexural Strength | 104 MPa | 15100 psi | ISO 178 |
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |