Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
IDI Composites 44-10 MW Thermoset Polyester, Molding Moderate strength material specifically formulated for microwave oven performance.Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
IDI Composites W-102 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Stratasys® Polycarbonate A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts .. |
|||
Flexural Strength | 97.1 MPa | 14100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® SC-1100R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 .. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 303V-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products a.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 302V-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products a.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 303-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Du-Co Ceramics DC-65 Cordierite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Flexural Strength | 97.2 MPa | 14100 psi | ASTM D790 |
Ensinger Tecapeek® XP-108 Compression Molded PEEK Compound, 20% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 97.2 MPa | 14100 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |