Mechanical Properties Metric English Comments
Flexural Strength 87.98 MPa
12760 psi
ASTM D790
Aclo Acculoy POL063L Polycarbonate PET Alloy
Flexural Strength 87.98 MPa
12760 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436G40CL Glass Reinforced