Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 79.6 MPa | 11500 psi | ASTM D790-03 |
Objet FullCure® 870 Vero Black Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ A6020 ASA+PC Available in North America Features: Good Impact Resistance and High Heat Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | |
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu.. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific) LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® VAC3003 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES HiFill® PBT 613 RD Availability: North AmericaForms: PelletsUL File Number: E157318Appearance: Red8661111Information provided by TP Composites, Inc. |
|||
Flexural Strength | 79.4 MPa | 11500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 79.4 MPa | 11500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Flexural Strength | 79.0 MPa @Thickness 3.17 mm |
11500 psi @Thickness 0.125 in |
chs 0.05 in/min; 2 in span; ASTM D790 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
Flexural Strength | 79.0 MPa @Strain 3.50 % |
11500 psi @Strain 3.50 % |
ISO 178 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D-790 |
Axiall 9209 Rigid PVC, Molding Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati.. |
|||
Flexural Strength | 79.0 MPa | 11500 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH325GK20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH325GK20 is a 10% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. It has a increased stiffness and a optimized warpage grade.Information .. |