Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87759 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |
|||
Flexural Strength | 69.6 MPa @Temperature 150 °C |
10100 psi @Temperature 302 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D790 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 69.5 MPa | 10100 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D790 |
Saint-Gobain Meldin® 3120 Thermoplastic Bearing Material 3120 is a multi-purpose, wear-resistant material is suitable for bearing, thrust washer, and piston ring applications. It also has a low coefficient of thermal expansion. Meldin® 3100 materials.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D-790 |
Axiall 3605 Rigid PVC, Extrusion, Natural Georgia Gulf 3605 is a special purpose compound formulated for the extrusion of thin wall profiles such as edge banding and furniture trim.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D-790 |
Axiall 3605 Rigid PVC, Extrusion, White Georgia Gulf 3605 is a special purpose compound formulated for the extrusion of thin wall profiles such as edge banding and furniture trim.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | |
Abatron AboCast 8503-7/AboCure 8503-7 Colorless Epoxy AboCast 8503-7/AboCure 8503-7 is a general purpose, slow hardening, colorless epoxy casting compound with low viscosity. It is similar to the 8503-4 system, but more flexible. Suggested Uses: Trans.. |
|||
Flexural Strength | 69.6 MPa | 10100 psi | ASTM D-790 |
Axiall 9202J Rigid PVC, Molding Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive produ.. |
|||
Flexural Strength | 69.6 MPa @Temperature 150 °C |
10100 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |