Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D-790 |
Plaskolite Optix® CA - 42 FDA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Multibase Nylex™ 2185 R20 Natural Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips MC3200 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | initial |
Malvern Minerals Nylon with Novacite® L-337 Quartz Filler Product data demonstrates the effect of the Novacite® (untreated lamellar quartz) filler. A separate entry demonstrates the effect of treated Novakup® filler in nylon. The specific nylon use.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 68.97 MPa | 10000 psi | ASTM D790 |
Lucent Polymers PC/PBT-0820 Polycarbonate+PBT, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | |
SGL Carbon Group EK 2240 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Techmer ES HiFill® HDPE E GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp CF006 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF006 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM Test |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |
|||
Flexural Strength | 68.9 - 124 MPa | 10000 - 18000 psi | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790-95 |
Multibase Multi-ABS 3632 High Heat Resistant Data provided by Multibase. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D-790 |
Axiall 3650 Rigid PVC, Extrusion Georgia Gulf 3650 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resistan.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific) LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Strength | >= 68.9 MPa | >= 10000 psi | |
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures Description: Master Bond Supreme 10HTND-3 features a blend of performance properties including both high shear and peel strengths along with a totally non-drip application feature. This one componen.. |