Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.0 - 79.0 MPa | 10900 - 11500 psi | ASTM D790 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |