Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 73.0 - 76.0 MPa | 10600 - 11000 psi | ASTM D790 |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Flexural Strength | 58.0 - 76.0 MPa @Strain 5.00 % |
8410 - 11000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |