Mechanical Properties Metric English Comments
Flexural Strength 2300 - 2800 MPa
334000 - 406000 psi
China Tungsten K520 Tungsten Carbide for Mining Purposes
High toughness, wear resistance and complex properties, for bits of hammer rock drills and heavy rock drills for cutting hard rocks.Information provided by China Tungsten
Flexural Strength 2350 - 2800 MPa
341000 - 406000 psi
China Tungsten Z30 Tungsten Carbide for Mining Purposes
High toughness and wear resistance and good versatility, for rotary hammer rock drill bits and heavy rock drill bits, for f16~f18 hard and medium hard rocks formationsInformation provided by China T..