Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 131 - 159 MPa | 19000 - 23000 psi | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Flexural Strength | 131 - 159 MPa | 19000 - 23000 psi | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Flexural Strength | 68.9 - 159 MPa | 10000 - 23000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Flexural Strength | 131 - 159 MPa | 19000 - 23000 psi | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Flexural Strength | 131 - 159 MPa | 19000 - 23000 psi | |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |