Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 116 - 143 MPa | 16800 - 20800 psi | |
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr.. |