Mechanical Properties Metric English Comments
Flexural Strength 8.30 - 10.3 MPa
1200 - 1490 psi
Ceradyne Thermo-Sil® Castable 120 Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..
Flexural Strength 6.90 - 10.3 MPa
1000 - 1490 psi
Ceradyne Thermo-Sil® Castable TG Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..