Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | >= 89.0 MPa | >= 12900 psi | |
MarkeTech Repton EXP 22 Magnesia MgO REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP LNP* THERMOCOMP* MX99432 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP (Asia Pacific) LNP* Thermocomp* MX99432 is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
Plenco 08112 Polyester BMC, Compression Molded PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
Polyplastics Duracon® M450-44/M450S Acetal Co-polymer (POM), Standard, Super high flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A2-9A Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A6-2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A7 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A7-7 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
Plenco 4311 Phenolic, Granular, Injection Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-11 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |
|||
Flexural Strength | 89.0 - 115 MPa | 12900 - 16700 psi | ASTM D790 |
3D Systems Accura® 10 Plastic for SLA® Systems Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsGeneral use prototyping for many uses, including:Enclosures, covers and casesCellular/mobile ph.. |