Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.3 MPa | 12400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 85.3 MPa | 12400 psi | 2.8 mm/min; ASTM D790 |