Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.0 MPa | 12300 psi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 BT N 29 B PA6 Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivered in the natu.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 BT N 29 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Flexural Strength | <= 85.0 MPa | <= 12300 psi | ISO 178 |
Polykemi AB POLYasa 3010F Extra High Flow ASA Information provided by Polykemi AB |
|||
Flexural Strength | 85.0 MPa @Temperature 23.0 °C |
12300 psi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**) Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 85.0 MPa @Temperature 23.0 °C |
12300 psi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Ineos Nova PS 3190 Crystal Polystyrene
(discontinued **) Information provided by Nova ChemicalsINEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2mm/min; ASTM D790 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-20 Polycarbonate, General Purpose Features: Standard, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformation .. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-30UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures/covers, Safety products, E & E parts, Household appl.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-40 Polycarbonate, General Purpose Features: Standard, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications, Le.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-40UV Polycarbonate, General Purpose, UV Stability Grade Features: UV stability, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
Lucite International Elvakon® 4474 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 1 mm/min; ISO 178 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Plenco 3557 Phenolic, Granular, Compression Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Polyram PlusTek PB840 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178-93 |
Wellman Wellamid® 22LHI3 XE-NBK1 Impact Modified Engineering Nylon 66 Description: Impact Modified Engineering Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | D790 |
Zhejiang Juner 301-G0 Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |