Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 84.81 MPa | 12300 psi | |
Abatron AboCast 8-6/Abocure 8-6 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 115 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |