Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 81.423 MPa | 11809 psi | |
Shinil Chemical SHINFLAME PC/ABS Flame Retardant Polymer TV Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |