Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES Electrablend® PEI 04008 MB Availability: North AmericaForms: PelletsFeatures: Conductive and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES Electrablend® POM CO Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and Medium ViscosityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES Luriblend® POM CO X MB Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
Flexural Strength | 81.4 MPa @Thickness 3.20 mm |
11800 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 202EL General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability Reduces processing cycle timeProcessing MoldingApplicationsAudio cassettes housing and covers, CD jewel boxes Medical products like disp.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D-790 |
Axiall 7450 Rigid PVC, Extrusion Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D790 |
Aremco Aremco-Bond™ 2150 High Performance Epoxide Ceramic-Filled, Fast-Setting, High Vibration Resistance and Bond Strength. Ideal for bonding ceramic wear tiles. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D-790 |
Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34 Georgia Gulf 8247 Clear 34 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and prote.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D-790 |
Axiall 8268 Rigid PVC, Extrusion Georgia Gulf 8268 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and protected jalo.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D-790 |
Axiall 9017 Rigid PVC, Molding Georgia Gulf 9017 is for food packaging applications requiring optimum taste and odor properties such as water and mouthwash.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | |
BCC Products BC 6128 Epoxy, Hi-Heat, Abrasion Resistant BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Ext.. |
|||
Flexural Strength | 81.4 MPa | 11800 psi | ASTM D-790 |
Axiall 9017J Clear 06 Rigid PVC, Molding, Clear Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects l.. |