Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 74.48 MPa | 10800 psi | ASTM D790 |
Lucent Polymers ABS-305 Acrylonitrile Butadiene Styrene, General Purpose Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 74.48 MPa | 10800 psi | ASTM D790 |
Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 74.48 MPa | 10800 psi | ASTM D790 |
Lucent Polymers ABS-45T Acrylonitrile Butadiene Styrene, High Impact Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |