Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | |
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | Stress at 5% Strain, Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1004 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
PolyOne Edgetek® AS-1000 Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:UnfilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Techmer ES HiFill® POM CO 0374 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Techmer ES Plaslube® PC-50/TF/13/SI/2 NAT Polycarbonate |
|||
Flexural Strength | 72.4 MPa @Thickness 3.17 mm |
10500 psi @Thickness 0.125 in |
ASTM D790 |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0877A 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-10FG-0100 10% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |