Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Techmer ES HiFill FR® ABS FR UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Techmer ES HiFill FR® ABS FR UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceUL File Number: E157318Appearance: BlackTPCI# 9224121Information provided by TP Compos.. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D 790 |
SABIC Innovative Plastics Noryl EBN90 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6 Information provided by A. Schulman. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6 Information provided by A. Schulman. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | |
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ISO 178 |
Unitika TERRAMAC TP-4030 Polylactic Acid (PLA) Soft, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-777E ABS - High Heat Ultra High Heat |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 102 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 71.0 MPa | 10300 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |